  1. What materials are subject to temper embrittlement?
    Low chrome material.

    Reference API 510: 3.1.69
  2. What material is subject to chloride stress-corrosion cracking?
    300 SS

    Reference API 571: 4.5.1.2.a
  3. What material is subject to polytheonic acid stress-corrosion cracking?
    300 SS (Austenitic SS)

    Reference API 572: 9.4.1
  4. What is a common material with an endurance limit? (Fatigue cracking cannot occur below this stress level)
    Carbon Steel.

    Reference API 571: 4.2.16.3.b.2
  5. What is a common material without an endurance limit?
    Austenitic SS

    300/400 SS, Aluminum, and most other non-ferrous alloys.

    Reference API 571: 4.2.16.3.b.2
  6. What P-numbers are allowed to use pre-heat in lieu of PWHT?
    P1 and P3

    Reference API 510: 8.1.7.4.3.2.1.a
  7. What P-numbers are allowed to use CDW (Controlled Deposition Welding) in lieu of PWHT?
    P1, P3, and P4.

    Reference API 510: 8.1.7.4.3.3.b
  8. P-numbers of a base metal that should be examined for delayed cracking after repairs to SS cladding?
    P3, P4, and P5.

    Reference API 510: 8.1.6.4.4

Card Set Information

Author:
Gibby
ID:
333627
Filename:
API 510 Data Sheets - Material - CLOSED BOOK QUESTIONS
Updated:
2017-08-22 01:47:02
Tags:
API 510
Folders:

Description:
MSTS Material CLOSED BOOK QUESTIONS
Show Answers:

Home > Flashcards > Print Preview